Steve
Mike2cl77 wrote:Thanks G-man, I have read through that post several times until my eyes burned. I did however find the recipe for the bath finally and ready to give it a try. However, how was I to know Communist Calif would make it so difficult for me to get Zinc. I will be in NorCal this weekend maybe they will have some MossBoss or something otherwise off to Ebay. In my readings I have read that temperature is a factor with plating, but I didn't see it mentioned in this forum. Did I miss something or have any of you dabbled with temperature?